MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Dow Appeel™ 52009 Ethylene Vinyl Acetate Copolymer
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Product Description: Appeel™ 52009 is a modified ethylene acid terpolymer resin designed to function as a sealing layer for lidding applications, most commonly sealing to foamed polystyrene. It is available in pellet form for use in conventional extrusion or coextrusion equipment designed to process polyethylene resins.
Uses:
  • Lidding Sealant
Applications:
  • Good heat sealability and easy peelability to foamed PS.
  • Excellent direct foil adhesion without the use of primers
  • Appeel 52009 conforms to Code #20 of the Ministry of health and Welfare Japan.

Typical structures for this lidding would be: Paper/PE/Foil/Appeel 52009. This product is used as a heat seal layer in lidding matieral for foamed PS, especially used in the packaging of instant noodle cup. It can also be used as a sealant in general flexible packaging. It provides low temperature seals for snacks and confectionery.

Availability: Africa & Middle East; Asia Pacific; Latin America; Europe; North America

Agency Ratings: FDA 21 CFR 177.1330 (b)

Form: Pellets

Processing Method: Coextrusion; Extrusion; Extrusion Coating

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.932 g/cc0.0337 lb/in³ASTM D792
Melt Flow 24 g/10 min
@Load 2.16 kg,
Temperature 190 °C
24 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Thermal PropertiesMetricEnglishComments
Melting Point 108 °C226 °FASTM D3418
Vicat Softening Point 63.9 °C147 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF397 / 311090

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.