MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Copper Alloy, UNS C48645, H02 Temper, Rod, Bar & Forging
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: 1/2 Hard

Good Suitability – Soldering, Brazing, Oxyacetylene Welding, Capacity for Being Hot Formed; Fair Suitability – Capacity for Being Cold Worked

Applicable Specifications: Rod, Bar & Forging – ASTM B21/B21M, ASTM B124/B124M, ASTM B283/B283M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.489 g/cc0.3067 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 50 - 8050 - 80
Tensile Strength 310 MPa45000 psi
Tensile Strength, Yield 103 MPa15000 psi0.5% Ext
Elongation at Break 20 %20 %
Tensile Modulus 93.1 GPa13500 ksi
Modulus of Rigidity 41.3 GPa5990 ksi
Poissons Ratio 0.330.33
Machinability 85 %85 %
Forgeability 90 %90 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000690 ohm-cm0.00000690 ohm-cm25% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 22.34 µm/m-°C
@Temperature 20.0 - 300 °C
12.41 µin/in-°F
@Temperature 68.0 - 572 °F
Thermal Conductivity 8.55 W/m-K59.3 BTU-in/hr-ft²-°F
Melting Point 868.3 - 893 °C1595 - 1640 °F
Solidus 868.3 °C1595 °F
Liquidus 893 °C1640 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 60 - 63 %60 - 63 %
Iron, Fe <= 0.30 %<= 0.30 %
Lead, Pb 1.0 - 2.5 %1.0 - 2.5 %
Nickel, Ni 0.10 - 1.0 %0.10 - 1.0 %
Phosphorus, P 0.020 - 0.25 %0.020 - 0.25 %
Tin, Sn 0.10 - 1.5 %0.10 - 1.5 %
Zinc, Zn 31.8 - 38.8 %31.8 - 38.8 %As Balance

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC48645x1 / 292057

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.