MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Ganpati Exim N326 Carbon Black
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Fine low-structure reinforcing carbon black. Provides low modulus, high elongation at break, high values of tear resistance and fatigue strength. Breaker compounds, including breaker compounds for giant and off-the-road tires. Conveyor belts, industrial rubber goods, seals.

Information provided by Ganpati Exim PVT. LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.445 - 0.485 g/cc0.0161 - 0.0175 lb/in³Pour
pH 6.0 - 8.06.0 - 8.0
Specific Surface Area 76 m²/g76 m²/gExternal; Statistical Thickness Surface Area,; ASTM D 6556
 78 - 88 m²/g78 - 88 m²/gExternal
Ash <= 0.45 %<= 0.45 %
 
Mechanical PropertiesMetricEnglishComments
300% Modulus 0.700 - 2.70 MPa102 - 392 psiIRB 6
 
Descriptive Properties
Carbon Black Temperature in a Hopper Car<65°C
Content<0.15%Toluene Extractables
 <1.1%Sulphur
DBP Absorption Number67-77 cm3/100g
DBP Absorption Number of Compressed Sample64-74 cm3/100g
Fines Content<7%Pelleted
Heating Loss<1.0%
Individual Pellet Hardness25-100 g
Iodine Number77-87 g/kg
Nitrogen Adsorption Number74-82 m2/g(D6556)
Sieve Residue<0.001%05
 <0.1%0045
Tint Index108-116%ITRB
Toluene Discoloration>90%transmittance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGANPATI003 / 317287

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.