MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
EOS Aluminum AlSi10Mg DMSL on EOS M 290; 60µm Layer Thickness
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Nonferrous Metal; Aluminum Alloy

Material Notes: Main Characteristics:
  • Good buildability
  • Good mechanical properties
  • High productivity
  • Heat treatment possible to improve ductility
Typical Applications: Higher productivity process can be used where mechanical requirements are less demanding but where cost-efficiency is needed. Heat treatment can be used to affect mechanical properties.

Heat Treatment: Solution annealing of 30 minutes in 530 °C followed by immediate quenching to water. Artificial aging of 6 hours in 165 °C followed by cooling in air.

Information provided by EOS GmbH (Electro Optical Systems).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Porosity 0.20 %
Thickness 60.0 microns
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 320 MPaheat treated
 440 MPaas manufactured
Tensile Strength, Yield 235 MPaas manufactured
 250 MPaheat treated
Elongation at Break 4.0 %as manufactured
 7.0 %
@Treatment Temp. 530 °C,
Time 1800 sec
heat treated
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 87.1 - 90.75 %Balance
Copper, Cu <= 0.050 %
Iron, Fe <= 0.55 %
Lead, Pb <= 0.050 %
Magnesium, Mg 0.25 - 0.45 %
Manganese, Mn <= 0.45 %
Nickel, Ni <= 0.050 %
Silicon, Si 9.0 - 11 %
Tin, Sn <= 0.050 %
Titanium, Ti <= 0.15 %
Zinc, Zn <= 0.10 %
 
Descriptive Properties
Surface roughness10 µmRa, Vertical
Volume rate10.5 mm3/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NEOS915 / 280575

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.