SABIC® PPcompound G3135X is a 35% short glass fiber reinforced Polypropylene. This material has been designed for high stiffness, high impact, high heat resistance and chemical resistance. The glass fibres are chemically coupled to the PP matrix. Typical application of this material would include air inlet manifolds. The material is available in standard black.
SABIC® PPcompound G3135X is a designated automotive grade.
IMDS ID: 136528620Information provided by SABIC |