MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EOS Flexline Aluminum AlSi10Mg DMSL on EOS M 290; 30µm Layer Thickness
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Nonferrous Metal; Aluminum Alloy

Material Notes: The alloy AlSi10Mg is characterized by good strength and hardness, as well as high dynamic load bearing capacity, and it therefore also used for parts subjected to high loads. It is typically used for cast parts with thin walls and complex geometry. Parts made of EOS Aluminum AlSi10Mg are ideal for applications that require a combination of good thermal properties and low weight. They can be machined, wire eroded and electrical discharge machined, welded, micro-blasted, polished and coated. Laser sintering process is extremely fast melting and re-solidification. Due to building in layers the parts have anisotropic properties. Suitable heat treatment can be used for further improvement of part properties and reduction of anisotropy. Conventionally cast components in this type of aluminum alloy are often heat treated to improve the mechanical properties, for example using the T6 cycle of solution annealing, quenching and age hardening.

Information provided by EOS GmbH (Electro Optical Systems).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.67 g/cc0.0965 lb/in³ISO 3369
Particle Size <= 90 µm<= 90 µm<0.5% larger
Thickness 30.0 microns1.18 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 440 - 480 MPa63800 - 69600 psiHorizontal, As-Manufactuered; ISO 6892-1 B10
 450 - 490 MPa65300 - 71100 psiVertical, As-Manufactuered; ISO 6892-1 B10
 340 MPa
@Treatment Temp. 270 °C,
Time 5400 sec
49300 psi
@Treatment Temp. 518 °F,
Time 1.50 hour
Annealed, Horizontal
 350 MPa
@Treatment Temp. 270 °C,
Time 5400 sec
50800 psi
@Treatment Temp. 518 °F,
Time 1.50 hour
Annealed, Vertical
Tensile Strength, Yield 210 - 250 MPa30500 - 36300 psiVertical, As-Manufactuered; ISO 6892-1 B10
 250 - 290 MPa36300 - 42100 psiHorizontal, As-Manufactuered; ISO 6892-1 B10
 220 MPa
@Treatment Temp. 270 °C,
Time 5400 sec
31900 psi
@Treatment Temp. 518 °F,
Time 1.50 hour
Annealed, Horizontal
 225 MPa
@Treatment Temp. 270 °C,
Time 5400 sec
32600 psi
@Treatment Temp. 518 °F,
Time 1.50 hour
Annealed, Vertical
Elongation at Break 4.0 - 8.0 %4.0 - 8.0 %Vertical, As-Manufactuered; ISO 6892-1 B10
 8.0 - 12 %8.0 - 12 %Horizontal, As-Manufactuered; ISO 6892-1 B10
 9.0 %
@Treatment Temp. 270 °C,
Time 5400 sec
9.0 %
@Treatment Temp. 518 °F,
Time 1.50 hour
Annealed, Vertical
 12 %
@Treatment Temp. 270 °C,
Time 5400 sec
12 %
@Treatment Temp. 518 °F,
Time 1.50 hour
Annealed, Horizontal
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 87.1 - 90.75 %87.1 - 90.75 %Balance
Copper, Cu <= 0.050 %<= 0.050 %
Iron, Fe <= 0.55 %<= 0.55 %
Lead, Pb <= 0.050 %<= 0.050 %
Magnesium, Mg 0.25 - 0.45 %0.25 - 0.45 %
Manganese, Mn <= 0.45 %<= 0.45 %
Nickel, Ni <= 0.050 %<= 0.050 %
Silicon, Si 9.0 - 11 %9.0 - 11 %
Tin, Sn <= 0.050 %<= 0.050 %
Titanium, Ti <= 0.15 %<= 0.15 %
Zinc, Zn <= 0.10 %<= 0.10 %
 
Descriptive Properties
Surface roughness50-100 µmRz after microblasting
 6-15 µmRa after microblasting
 70-120 µmRz as manufacture
 9-20 µmRa as manufacture
Volume rate5.1 mm³/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NEOS914 / 280574

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.