MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chemours Krytox™ GPL 246 PFPE Electrical Conducting Grease
Categories: Fluid; Lubricant; Perfluoropolyether (PFPE)

Material Notes: Formulated with copper powder in grease to act as a conductor of electricity. Krytox™ oils provide long life and high-temperature stability and lubrication. The addition of copper powder also improves the thermal conductivity of the grease for applications where improved heat transfer is needed; however, it can increase bearing noise and wear. Thermal conductivity of non-additive Krytox™ GPL 206 grease at 40 °C (104 °F) is 0.127 watts/mK. The Krytox™ GPL 246 grease at 40 °C (104 °F) has conductivity of 0.272 watts/mK. Because Krytox™ GPL 246 is formulated with Krytox™ GPL 106 base oil, it retains many of the properties of that oil.

Information provided by Chemours Krytox

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measure  25 cSt
@Temperature 100 °C
25 cSt
@Temperature 212 °F
base oil
 240 cSt
@Temperature 40.0 °C
240 cSt
@Temperature 104 °F
base oil
 810 cSt
@Temperature 20.0 °C
810 cSt
@Temperature 68.0 °F
base oil
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 35000 ohm-cm35000 ohm-cmASTM D257
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.272 W/m-K
@Temperature 40.0 °C
1.89 BTU-in/hr-ft²-°F
@Temperature 104 °F
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -36.0 °C-32.8 °F
 
Descriptive Properties
AppearanceCopper colored, buttery
Standard NLGI Grade2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WDUPJ836 / 254024

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.