Ultramid Advanced N4H is an unfilled partially aromatic polyphthalamide for injection molding and extrusion with strong mechanical properties especially at elevated temperatures, good long-term thermal stability and excellent chemical resistance for highly stressed parts. This material has high toughness, extremely low water absorption, outstanding dimensional stability and very good wear/sliding friction properties. It features a high melting point (300C) and excellent melt stability.Information provided by BASF. |