System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
SABIC LNP™ LUBRICOMP™ Compound OFL36XXC Polyphenylene Sulfide, Linear (PPS, Linear)
Categories:
Polymer
;
Thermoplastic
;
Polyphenylene Sulfide (PPS)
Material Notes:
LNP LUBRICOMP OFL36XXC compound is based on Polyphenylene Sulfide (PPS) - linear resin containing 30% glass fiber, 15% PTFE. Added features of this grade include: Wear Resistant.
Features: Wear resistant,Structural
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.69
g/cc
0.0611
lb/in³
ASTM D792
1.70
g/cc
0.0614
lb/in³
ISO 1183
Moisture Absorption
0.0100 %
0.0100 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow
0.0010
-
0.0020
cm/cm
0.0010
-
0.0020
in/in
24hrs; ASTM D955
0.0013
-
0.0018
cm/cm
0.0013
-
0.0018
in/in
24hrs; ISO 294
Linear Mold Shrinkage, Transverse
0.0030
-
0.0048
cm/cm
0.0030
-
0.0048
in/in
24hrs; ISO 294
0.0060
-
0.0080
cm/cm
0.0060
-
0.0080
in/in
24hrs; ASTM D955
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
121
MPa
17500
psi
5 mm/min; ISO 527
124
MPa
18000
psi
5 mm/min; ASTM D638
Elongation at Break
1.3 %
1.3 %
5 mm/min; ASTM D638
1.3 %
1.3 %
5 mm/min; ISO 527
Tensile Modulus
11.99
GPa
1739
ksi
1 mm/min; ISO 527
12.8
GPa
1860
ksi
50 mm/min; ASTM D638
Flexural Strength
178
MPa
25800
psi
brk, 1.3 mm/min, 50 mm span; ASTM D790
180
MPa
26100
psi
ISO 178
Flexural Modulus
11.05
GPa
1603
ksi
2 mm/min; ISO 178
11.6
GPa
1680
ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched
60.0
J
44.3
ft-lb
ASTM D256
Izod Impact, Unnotched
4.16
J/cm
7.79
ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO)
5.00
kJ/m²
2.38
ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO)
24.0
kJ/m²
11.4
ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy
3.00
J
2.21
ft-lb
peak; ASTM D3763
11.0
J
8.11
ft-lb
ASTM D3763
Impact Test
2.00
J
1.48
ft-lb
Multiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic
0.44
0.44
ASTM D3702 Modified: Manual
Coefficient of Friction, Static
0.35
0.35
ASTM D3702 Modified: Manual
K (wear) Factor
14.1
-
16.1
x 10
-8
mm³/N-M
7.00
-
8.00
x 10
-10
in³-min/ft-lb-hr
Ring; ASTM D3702 Modified: Manual
105
x 10
-8
mm³/N-M
52.0
x 10
-10
in³-min/ft-lb-hr
Washer; ASTM D3702 Modified: Manual
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
23.0
µm/m-°C
@Temperature -40.0 - 40.0 °C
12.8
µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
24.0
µm/m-°C
@Temperature -40.0 - 40.0 °C
13.3
µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
25.0
µm/m-°C
@Temperature -30.0 - 30.0 °C
13.9
µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
CTE, linear, Transverse to Flow
34.0
µm/m-°C
@Temperature -30.0 - 30.0 °C
18.9
µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
48.0
µm/m-°C
@Temperature -40.0 - 40.0 °C
26.7
µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
50.0
µm/m-°C
@Temperature -40.0 - 40.0 °C
27.8
µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi)
278
°C
532
°F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
278
°C
@Thickness 3.20 mm
532
°F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
257
°C
495
°F
Flatw 80*10*4 sp=64mm; ISO 75/Af
264
°C
@Thickness 3.20 mm
507
°F
@Thickness 0.126 in
unannealed; ASTM D648
UL RTI, Electrical
105
°C
221
°F
UL 746B
UL RTI, Mechanical with Impact
105
°C
221
°F
UL 746B
UL RTI, Mechanical without Impact
105
°C
221
°F
UL 746B
Flammability, UL94
V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
UL 94
Processing Properties
Metric
English
Comments
Zone 2
320
-
330
°C
608
-
626
°F
Zone 3
330
-
345
°C
626
-
653
°F
Melt Temperature
315
-
320
°C
599
-
608
°F
Injection Molding
Mold Temperature
140
-
165
°C
284
-
329
°F
Drying Temperature
120
-
150
°C
248
-
302
°F
Injection Molding
Dry Time
4.00
hour
4.00
hour
Injection Molding
Back Pressure
0.200
-
0.300
MPa
29.0
-
43.5
psi
Screw Speed
30
-
60
rpm
30
-
60
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PSABH80927 / 288874
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.