MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC NORYL™ Resin NH5020 Polyphenylene Ether + PS (PPE+PS) (Europe)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ NH5020 resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade contains non-brominated, non-chlorinated flame retardant and exhibits high heat resistance with thin-wall FR performance. NORYL NH5020 resin carries a UL94 flame rating of V0 at 0.75mm along with a UL746C Outdoor Suitability rating of F1. The material offers a good balance of affordable high heat, flow, hydrolytic stability, excellent creep resistance, dimensional stability and is a good candidate for photovoltaic / solar connectors, UPS Inverters / chargers, and outdoor enclosure applications.

Features: Hydrolytic Stability,Low Creep Sensitivity,Flame Retardant,Non-Halogenated,Non-Chlorinated,Non-Brominated,Low Warpage

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/ccASTM D792
Density 1.11 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
 0.0500 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.25 %ISO 62-1
Viscosity 10 cP
@Load 5.00 kg,
Temperature 280 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 9.8 g/10 min
@Load 5.00 kg,
Temperature 280 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 62.0 MPa50 mm/min; ASTM D638
 77.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 79.0 MPa50 mm/min; ASTM D638
 80.0 MPa50 mm/min; ISO 527
Elongation at Break 5.6 %50 mm/min; ISO 527
 15 %50 mm/min; ASTM D638
Elongation at Yield 4.7 %50 mm/min; ISO 527
 5.0 %50 mm/min; ASTM D638
Tensile Modulus 2720 MPa50 mm/min; ASTM D638
 3050 MPa1 mm/min; ISO 527
Flexural Strength 122 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
 126 MPayield, 2 mm/min; ISO 178
Flexural Modulus 2980 MPa2 mm/min; ISO 178
 3000 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 91.0 JASTM D256
 59.0 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 8.00 kJ/m²80*10*4; ISO 180/1A
 6.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 7.00 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 19.0 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 49.0 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
Arc Resistance 60 - 120 secASTM D495
Comparative Tracking Index 250 - 400 VUL 746A
Hot Wire Ignition, HWI >= 120 sec
@Thickness >=0.750 mm
UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness >=0.750 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 61.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 61.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 68.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 68.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Hot Ball Pressure Test 125 °CPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 122 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 133 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 119 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 117 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 122 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 137 °CRate B/50; ASTM D1525
 138 °CRate B/50; ISO 306
 139 °CRate B/120; ISO 306
UL RTI, Electrical 110 °CUL 746B
UL RTI, Mechanical with Impact 105 °CUL 746B
UL RTI, Mechanical without Impact 110 °CUL 746B
Flammability, UL94 V-2
@Thickness >=0.400 mm
UL 94
 V-0
@Thickness >=0.750 mm
UL 94
 5VA
@Thickness >=2.50 mm
UL 94
Glow Wire Ignition Temperature 775 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 275 - 305 °C
Zone 2 255 - 300 °C
Zone 3 265 - 305 °C
Melt Temperature 275 - 305 °CInjection Molding
Mold Temperature 70.0 - 100 °C
Drying Temperature 105 - 110 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 30 - 70 %
Vent Depth 0.00380 - 0.00510 cm
Screw Speed 20 - 100 rpm
 
Descriptive Properties
UV-light, water exposure/immersionF1UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82386 / 290333

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.