MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Angst+Pfister APSOplast® VESPEL PI SP21 PI + 15% graphite
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic; Thermoplastic Polyimide, Graphite Filled

Material Notes: The 15% graphite content improves the coefficient of friction, wear resistance, and heat ageing. This type is suitable for lubricated and non-lubricated applications which require low friction and wear properties.

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.51 g/cc0.0546 lb/in³DIN EN ISO 1183-1
Moisture Absorption 1.10 %1.10 %at saturation in standardized climate; DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 66.0 MPa9570 psiASTM D 1708
Elongation at Break 4.5 %4.5 %ASTM D 1708
Modulus of Elasticity 3.79 GPa550 ksiASTM D 790
Izod Impact, Notched 0.427 J/cm0.800 ft-lb/inASTM D 256
Izod Impact, Unnotched 3.20 J/cm5.99 ft-lb/inASTM D 256
Coefficient of Friction 0.300.30p=0.05 N/mm2, v=0.6 m/s, against hardened and polished steel
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 - 1.00e+13 ohm-cm1.00e+12 - 1.00e+13 ohm-cmASTM D 257
Dielectric Constant 13.53
@Frequency 100 Hz
13.53
@Frequency 100 Hz
ASTM D 150
Dielectric Strength 9.84 kV/mm250 kV/inASTM D 149
Dielectric Loss Index 0.0053
@Frequency 100 Hz
0.0053
@Frequency 100 Hz
ASTM D 150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 49.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
27.2 µin/in-°F
@Temperature 73.4 - 140 °F
Thermal Conductivity 0.870 W/m-K6.04 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 300 °C572 °Flong term
 360 °C680 °Fshort term
Deflection Temperature at 1.8 MPa (264 psi) 360 °C680 °FDIN EN ISO 75 / A
Flammability, UL94 V-0V-0
 
Descriptive Properties
Coloranthracite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PANGP071 / 250569

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.