MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Danquinsa MORCHEM AQ 710 + CA-15 Adhesive
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: MORCHEM AQ 710 + CA-15 is a two component adhesive based on polyurethane water dispersion.

Application: MORCHEM AQ 710 + CA-15 provides good bonding properties on most synthetic and natural materials (fabrics, PVC…). The adhesive can be used as one component when high performance is not required. The addition of the component MORCHEM CA-15 increases washing resistance. MORCHEM AQ 710 + CA-15 is a water based dispersion with low VOC content. The product presents good yellowing resistance properties. The use of MORCHEM AQ 710 + CA-15 gives a good soft hand feel. MORCHEM AQ 710 + CA-15 is a thermoplastic adhesive heat-activated at 75- 80°C.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 - 1.07 g/ccMORCHEM AQ 710
 1.13 - 1.17 g/ccMORCHEM CA-15
Solids Content 38 - 42 %MORCHEM AQ 710
 100 %MORCHEM CA-15
pH 7.0 - 9.5MORCHEM AQ 710
Brookfield Viscosity 105 - 315 cPMORCHEM CA-15
 3000 - 5500 cPMORCHEM AQ 710
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
 
Descriptive Properties
AspectMilky whiteMORCHEM AQ 710
 TransparentMORCHEM CA-15

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDANQ184 / 294604

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.