MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ravago Manufacturing Americas Hylon® N2040MHL BK Nylon 6, 40% Mineral Reinforced, Heat Stabilized, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 40% Mineral Filled; Nylon 6, Heat Stabilized

Material Notes: Product Description: PA 6, 40% Mineral Reinforced, Heat Stabilized, Lubricated, Black Color

Availability: North America

Filler/Reinforcement: Mineral, 40% Filler by Weight

Additive: Heat Stabilizer; Lubricant

Features: Heat Stabilized; Lubricated

Uses: Automotive Applications

RoSH Compliance: RoSH Compliant

Automotive Specifications: CHRYSLER MS.50017 MS-DB-41 CPN2931

Appearance: Black

Information provided by Ravago Manufacturing Americas

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.49 g/cc0.0538 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 50.0 MPa7250 psiISO 527-2
Elongation at Break 5.0 %5.0 %ISO 527-2
Flexural Strength 52.0 MPa7540 psiISO 178
Flexural Modulus 2.87 GPa416 ksiISO 178
Izod Impact, Notched (ISO) 6.93 kJ/m²3.30 ft-lb/in²ISO 180
Charpy Impact, Notched 0.693 J/cm²3.30 ft-lb/in²ISO 179

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRAVAGO41098 / 311791

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.