MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC GELOY™ XP4045LG ASA (Americas)
Categories: Polymer; Thermoplastic; ASA Polymer

Material Notes: PC/ASA. Excellent weatherability, low gloss.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0060 - 0.0090 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0060 - 0.0090 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 28 g/10 min
@Load 5.00 kg,
Temperature 260 °C
cm³/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 45.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 60.0 MPa50 mm/min; ISO 527
Elongation at Break 46.7 %50 mm/min; ISO 527
Elongation at Yield 5.2 %50 mm/min; ISO 527
Tensile Modulus 2320 MPa1mm/min; ISO 527
Flexural Yield Strength 93.0 MPa2 mm/min; ISO 178
Flexural Modulus 2270 MPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) 14.0 kJ/m²80*10*4; ISO 180/1A
 8.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
 8.00 kJ/m²
@Temperature -40.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 25.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 12.0 kJ/m²
@Temperature -40.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
 14.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 45.0 Jpeak; ASTM D3763
 53.0 JASTM D3763
 15.0 J
@Temperature -30.0 °C
peak; ASTM D3763
 17.0 J
@Temperature -30.0 °C
ASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 67.0 µm/m-°C
@Temperature -30.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 76.0 µm/m-°C
@Temperature -30.0 - 80.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 125 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 103 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
Vicat Softening Point 126 °CRate B/50; ISO 306
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 260 - 275 °CInjection Molding
Zone 1 260 - 280 °C
Zone 2 250 - 275 °C
Zone 3 240 - 270 °C
Melt Temperature 265 - 285 °C
Mold Temperature 50.0 - 80.0 °C
Drying Temperature 95.0 - 105 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
Moisture Content 0.040 %
Back Pressure 0.300 - 1.00 MPa
Shot Size 40 - 80 %
Vent Depth 0.00380 - 0.00760 cm
Screw Speed 30 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10153 / 243620

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.