MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultradur® B 4040 G3 FR BK7696 PBT/PET, 15% Glass Fiber Reinforced, Flame Retardant
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); PBT + PET Blend, Glass Filled

Material Notes: Product Description: Ultradur® B 4040 G3 FR BK7696 is a 15% glass filled, pigmented black, injection molding, flame retarded PBT + PET product. The product is intended for houses hold appliances where good chemical resistance, heat resistance and flame retardancy are required. The product also exhibits good surface appearance. Applications include oven and range top components, exterior parts for deep fryers, toasters, coffee machines, steam irons and cooker knobs and handles.

Availability: North America

Filler/Reinforcement: Glass Fiber, 15% Filler by Weight

Features: Chemical Resistant; Flame Retardant; Good Heat Resistance; Good Surface Finish

Use: Appliances

Agency Ratings: EC 1907/2006 (REACH)

RoSH Compliance: RoSH Compliant

Appearance: Black

Form: Pellets

Processing Method: Injection Molding

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.56 g/cc0.0564 lb/in³ISO 1183
Maximum Moisture Content 0.0150.015
Melt Flow 28 g/10 min
@Load 2.16 kg,
Temperature 265 °C
28 g/10 min
@Load 4.76 lb,
Temperature 509 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 86.9 MPa12600 psiISO 527-2
Elongation at Break 1.5 %1.5 %ISO 527-2
Tensile Modulus 7.03 GPa1020 ksiISO 527-1
Flexural Modulus 6.80 GPa986 ksiISO 178
Charpy Impact Unnotched 2.10 J/cm²10.0 ft-lb/in²ISO 179
Charpy Impact, Notched 0.504 J/cm²2.40 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 157 °C315 °FUnannealed; ISO 75-2/A
UL RTI, Electrical  140 °C
@Thickness 1.52 mm
284 °F
@Thickness 0.0600 in
UL 746B
 140 °C
@Thickness 3.05 mm
284 °F
@Thickness 0.120 in
UL 746B
UL RTI, Mechanical with Impact  130 °C
@Thickness 1.52 mm
266 °F
@Thickness 0.0600 in
UL 746B
 130 °C
@Thickness 3.05 mm
266 °F
@Thickness 0.120 in
UL 746B
UL RTI, Mechanical without Impact  130 °C
@Thickness 1.52 mm
266 °F
@Thickness 0.0600 in
UL 746B
 130 °C
@Thickness 3.05 mm
266 °F
@Thickness 0.120 in
UL 746B
Flammability, UL94  V-0
@Thickness 1.52 mm
V-0
@Thickness 0.0600 in
 V-0
@Thickness 3.05 mm
V-0
@Thickness 0.120 in
 5VA
@Thickness 3.05 mm
5VA
@Thickness 0.120 in
 5VA
@Thickness 1.52 mm
5VA
@Thickness 0.0600 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 275 °C464 - 527 °F
Mold Temperature 60.0 - 100 °C140 - 212 °F
Drying Temperature 100 - 120 °C212 - 248 °F
Dry Time 4.00 hour4.00 hour
Injection Pressure 3.50 - 12.5 MPa508 - 1810 psi
Back Pressure <= 1.00 MPa<= 145 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASG2148 / 310841

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.