MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Resinoid 2277 Phenolic Molding, Cellulose Reinforced
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Cellulose Filled

Material Notes: Data provided by the manufacturer.

Resinoid 2277 is a chopped fabric reinforced, two-step phenolic molding compound. It was specifically developed for molding applications where a lightweight, high strength material with good impact strength is needed. This material comes in pelletized from and is suitable for transfer or compression molding and can be used in injection molding systems with deep flight screws. Resinoid 2277 meets the requirements of ASTM D-5948 CFI-20 (Formerly MIL M14/1 CFI-20).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccASTM D792A
Water Absorption 0.80 %24 HR. R.T.; ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 41.0 MPaASTM D651
Flexural Strength 90.0 MPaASTM D790
Flexural Modulus 9.00 GPaASTM D790
Compressive Strength 153 MPaASTM D695
Izod Impact, Notched 0.680 J/cmASTM D256A
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 12.6 kV/mmASTM D149
Arc Resistance 125 secASTM D495
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-01/4”
 
Descriptive Properties
ColorBlack
FormPellet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPHR0WA / 253986

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.