Product Description: PBF3500J is a medium impact copolymer of polypropylene designed for such application as dairy packaging, deli-containers and stadium cups. It is characterized by easy mold flow, excellent physical property balance and finished product dimensional stability. Applications: - Compound
- Thin-wall Injection Molding
Information provided by CIPLAS by ITOCHU |