MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
SABIC LNP™ THERMOCOMP™ PDXE00715EES PEI (Americas)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: LNP Thermocomp PDXE00715EES is a compound based on PEI containing proprietary fillers. Added feature of this grade: Healthcare.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.36 g/ccASTM D792
Density 1.35 g/ccASTM D792
Moisture Absorption 0.170 %50% RH, 24 hrs; ASTM D570
 0.290 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.023 cm/cm
@Time 86400 sec
ASTM D955
Linear Mold Shrinkage, Transverse 0.024 cm/cm
@Time 86400 sec
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 123 MPa5 mm/min; ISO 527
 129 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 127 MPa5 mm/min; ISO 527
 129 MPa5 mm/min; ASTM D638
Elongation at Break 5.8 %5 mm/min; ISO 527
 6.0 %5 mm/min; ASTM D638
Elongation at Yield 4.5 %5 mm/min; ISO 527
 4.7 %5 mm/min; ASTM D638
Tensile Modulus 4986 MPa1mm/min; ISO 527
 5022 MPa5 mm/min; ASTM D638
Flexural Strength 202 MPaISO 178
Flexural Modulus 5084 MPa2 mm/min; ISO 178
 5090 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 52.9 J/mASTM D256
Izod Impact, Unnotched 687 J/mASTM D4812
Izod Impact, Notched (ISO) 5.20 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 37.2 kJ/m²80*10*4; ISO 180/1U
Impact Test 2.20 JMultiaxial Impact; ISO 6603
 7.10 JMultiaxial Impact; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 32.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
CTE, linear, Transverse to Flow 46.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 213 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 211 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 205 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 205 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Zone 1 343 - 354 °C
Zone 2 354 - 365 °C
Zone 3 365 - 376 °C
Melt Temperature 360 - 365 °C
Mold Temperature 121 - 148 °C
Drying Temperature 121 °CInjection Molding
Dry Time 4.00 - 6.00 hourCumulative; Injection Molding
Moisture Content 0.020 %
Back Pressure 0.340 - 0.680 MPa
Screw Speed 60 - 100 rpm

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI13775 / 247242

Ensinger SPI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.