MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SACO AEI PEXIDAN® L/T Eclipse Various Colors Curable Polyethylene Compound
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Description: PEXIDAN® L/T (including L/T-UV and L/T Eclipse) is a high density PEX system consisting of a silane grafted base compound A-1001 and a catalyst masterbatch CAT-003 (or A-1022 and CAT-117). When mixed and extruded in the proper proportions, the two-component system results in a material that is crosslinkable by exposure to moisture or by immersion in hot water at 90-95°C. PEXIDAN® L/T is listed by NSF International to standards 14 and 61 and to Canadian Standards Association standard B137.5. NSFI certification to ASTM F876 and ASTM F2023 testifies to its superior resistance to oxidation by hot, chlorinated water. PEXIDAN® L/T is permitted to be used in domestic continuous re-circulation systems and is listed by NSF as a NSF-pw CL5 / PEX 5006 material.

Typical values reported above (except MFR) are obtained from samples cured in hot water (6 hours @ 95°C).

Information provided by SACO AEI Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.946 g/ccASTM D792
Oxidative Induction Time (OIT) >= 50 min
@Temperature 220 °C
ASTM D3895
Melt Flow 0.70 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Storage Temperature <= 30.0 °F
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 3425 psiASTM D638
 1740 psi
@Temperature 82.0 °C
ASTM D638
 1740 psi
@Temperature 93.0 °C
ASTM D638
Tensile Strength, Yield 3100 psiASTM D638
 1260 psi
@Temperature 93.0 °C
ASTM D638
 1625 psi
@Temperature 82.0 °C
ASTM D638
Elongation at Break 0.00 %Hot, Permanent elongation (set) after cooling; SACO AEI DWI-QA-4007 based on ICEA T-28-562
 240 %ASTM D638
 200 %
@Temperature 82.0 °C
ASTM D638
 240 %
@Temperature 93.0 °C
ASTM D638
 30 %
@Temperature 150 °C,
Time 900 sec
Hot, Elongation under 0.2 N/mm2 load; SACO AEI DWI-QA-4007 based on ICEA T-28-562
Elongation at Yield 9.0 %ASTM D638
 12 %
@Temperature 82.0 °C
ASTM D638
 14 %
@Temperature 93.0 °C
ASTM D638
Tensile Modulus 125000 psi
@Temperature 23.0 °C
ISO 527
 245000 psi
@Temperature 0.000 °C
ISO 527
 335000 psi
@Temperature -40.0 °C
ISO 527
Flexural Modulus 30000 psi
@Temperature 23.0 °C
elastic; ISO 178
 55000 psi
@Temperature 0.000 °C
elastic; ISO 178
 75000 psi
@Temperature -40.0 °C
elastic; ISO 178
 
Thermal PropertiesOriginal ValueComments
CTE, linear 150 µm/m-°C
@Temperature -100 - 85.0 °C
ASTM D696
Specific Heat Capacity 1.92 J/g-°C
Vicat Softening Point 124 °CASTM D1525
 
Processing PropertiesOriginal ValueComments
Processing Temperature 320 - 350 °Fbarrel zones
Die Temperature 365 °F
Head Temperature 365 °F
 
Descriptive Properties
Degree of Crosslinking70%ASTM D2765

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSACO045 / 249412

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.