MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Master Bond LED405FL3 One component, flexibilized LED curable system
Categories: Polymer; Thermoset

Material Notes: Master Bond LED405FL3 is a one part system that cures upon exposure to LED light at 405 nm. It will cure rapidly and fully without any oxygen inhibition. Significantly, a UV light source is not needed to achieve polymerization. The speed of cure depends upon the intensity of the light source, the thickness of the layer, and the distance of the light source from the material being cured. The intensity of the light should be 2-4 watts/cm2. Thinner sections will typically cure in 30-45 seconds. Thicker sections will take longer. LED405FL3 bonds well to a wide variety of substrates including plastics, glass and metals. A salient feature is its flexibility, which allows the system to be compatible for bonding materials with different coefficients of thermal expansion. Additionally, it can withstand rigorous thermal cycling, mechanical shock and vibration. It is a reliable electrical insulator with a service temperature range of -100°F to 250°F. LED405FL3 resists many chemicals including mild acids, bases, oils, fuels and water. In fact, a cured sample withstood 12 hours of immersion in hot water (90°C) without any significant change in weight. The system is a good candidate for applications in aerospace, opto-electrical, optical, and specialty OEM, where a strong, flexible LED curable system is desirable.

Product Advantages:

  • One component system, needs no mixing
  • Cures by LED light, UV light not required
  • Superb flexibility, withstands thermal cycling
  • Can be used for small pottings and encapsulation
  • Especially resistant to water
Key Features:
  • Fast cure with appropriate LED light
  • Not oxygen inhibited
  • Outstanding optical clarity, with fluorescent dye
  • Can cure up to 1/8 inch thick

Information provided by Master Bond.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 500 - 3000 cP500 - 3000 cP
Linear Mold Shrinkage 0.010 cm/cm0.010 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5.0 - 155.0 - 15
Tensile Strength 6.89 - 13.8 MPa1000 - 2000 psi
Tensile Modulus 0.172 - 0.345 GPa25.0 - 50.0 ksi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm
Dielectric Constant 4.5
@Frequency 60 Hz
4.5
@Frequency 60 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 120 - 140 µm/m-°C66.7 - 77.8 µin/in-°F
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -73.0 °C-99.4 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.511.51
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 - 6.00 Month3.00 - 6.00 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMASTM642 / 268830

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.