LNP STAT-KON OE008A compound is based on Polyphenylene Sulfide (PPS) branched resin containing 40% carbon fiber. Added features of this grade include: Electrically Conductive. Features: High Stiffness,Light-weight Structural,Super Strong (Carbon Fiber Filled),Electrically Conductive Information provided by SABIC |