MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ STAT-LOY™ Compound N30009 Polycarbonate + ABS (PC+ABS) (Americas)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: LNP STAT-LOY N30009 compound is based on Polycarbonate/Acrylonitrile Butadiene Styrene (PC/ABS) blend containing proprietary fillers. Added features of this grade include: Permanently Anti-Static, Flame Retardant.

Features: Flame Retardant,Antistatic

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.26 g/cc0.0455 lb/in³ASTM D792
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Linear Mold Shrinkage, Flow 0.0053 - 0.0065 cm/cm0.0053 - 0.0065 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0053 - 0.0065 cm/cm0.0053 - 0.0065 in/in24hrs; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 49.0 MPa7110 psiASTM D638
Tensile Strength, Yield 55.0 MPa7980 psiASTM D638
Elongation at Break 100 %100 %ASTM D638
Elongation at Yield 5.0 %5.0 %ASTM D638
Tensile Modulus 2.15 GPa312 ksi50 mm/min; ASTM D638
Flexural Strength 84.0 MPa12200 psiASTM D790
Flexural Modulus 2.15 GPa312 ksiASTM D790
Izod Impact Notched 640 J472 ft-lbASTM D256
Dart Drop, Total Energy 38.0 J28.0 ft-lbpeak; ASTM D3763
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+10 - 1.00e+12 ohm1.00e+10 - 1.00e+12 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
@Thickness 3.20 mm
212 °F
@Thickness 0.126 in
unannealed; ASTM D648
UL RTI, Electrical 60.0 °C140 °FUL 746B
UL RTI, Mechanical with Impact 60.0 °C140 °FUL 746B
UL RTI, Mechanical without Impact 60.0 °C140 °FUL 746B
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Zone 2 210 - 220 °C410 - 428 °F
Zone 3 220 - 230 °C428 - 446 °F
Melt Temperature 200 - 230 °C392 - 446 °FInjection Molding
Mold Temperature 40.0 - 55.0 °C104 - 131 °F
Drying Temperature 80.0 °C176 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81419 / 289366

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.