MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Zytel® 158L NC010 Nylon 612  (Unverified Data**)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612)

Material Notes: Unreinforced Polyamide 612

This product line has been acquired from DuPont by Celanese. This specific page is outdated and not maintained. If the product is active, it can be found under its current Celanese listing.

Key Words: PA612
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/cc
 1.06 g/ccDAM; ISO 1183
Water Absorption 3.0 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Moisture Absorption 1.30 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Viscosity Test 120 cm³/gDAM; ISO 307 1157 1628
Linear Mold Shrinkage, Flow 0.013 cm/cmDAM; ISO 294-4 2577
 0.011 cm/cm
@Thickness 3.20 mm
DAM
Linear Mold Shrinkage, Transverse 0.014 cm/cmDAM; ISO 294-4 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 52.0 MPa50%RH; ISO 527-1/-2
 62.0 MPaDAM; ISO 527-1/-2
Elongation at Break 35 %DAM; Nominal; ISO 527-1/-2
 >= 50 %50%RH; Nominal; ISO 527-1/-2
Elongation at Yield 4.5 %DAM; ISO 527-1/-2
 19 %50%RH; ISO 527-1/-2
Tensile Modulus 1500 MPa50%RH; ISO 527-1/-2
 2400 MPaDAM; ISO 527-1/-2
Flexural Modulus 1450 MPa50%RH; ISO 178
 2050 MPaDAM; ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²DAM; ISO 180/1A
 6.00 kJ/m²50%RH; ISO 180/1A
 4.00 kJ/m²
@Temperature -30.0 °C
50%RH; ISO 180/1A
 5.00 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
Charpy Impact Unnotched NBDAM; ISO 179/1eU
 NB50%RH; ISO 179/1eU
 NB
@Temperature -30.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched 4.00 kJ/m²DAM; ISO 179/1eA
 6.00 kJ/m²50%RH; ISO 179/1eA
 4.00 kJ/m²
@Temperature -30.0 °C
50%RH; ISO 179/1eA
 5.00 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmDAM; IEC 60093
Surface Resistance >= 1.00e+15 ohm50%RH; IEC 60093
Dielectric Constant 3.2
@Frequency 1e+6 Hz
DAM; IEC 60250
 3.6
@Frequency 100 Hz
DAM; IEC 60250
Dielectric Strength 36.0 kV/mmDAM; IEC 60243-1
 36.0 kV/mm50%RH; IEC 60243-1
Dissipation Factor 0.014
@Frequency 100 Hz
DAM; IEC 60250
 0.016
@Frequency 1e+6 Hz
DAM; IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 120 µm/m-°CDAM; ISO 11359-1/-2
 90.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
DAM; ISO 11359-1/-2
 170 µm/m-°C
@Temperature 55.0 - 160 °C
DAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 120 µm/m-°CDAM; ISO 11359-1/-2
 90.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
DAM; ISO 11359-1/-2
 180 µm/m-°C
@Temperature 55.0 - 160 °C
DAM; ISO 11359-1/-2
Specific Heat Capacity 2.80 J/g-°C
Thermal Conductivity 0.190 W/m-Kof melt
Melting Point 218 °CDAM; 10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 135 °CDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °CDAM; ISO 75-1/-2
Glass Transition Temp, Tg 60.0 °CDAM; 10°C/min; ISO 11357-1/-2
Flammability, UL94 HB
@Thickness 1.50 mm
DAM; IEC 60695-11-10
 HB
@Thickness 0.900 mm
DAM; IEC 60695-11-10
Oxygen Index 25 %DAM; ISO 4589-1/-2
 
Descriptive Properties
AdditivesLubricants
 Release agent
Delivery formPellets
Part Marking Code>PA612<ISO 11469
ProcessingCasting
 Coatable
 Film Extrusion
 Injection Molding
 Other Extrusion
 Profile Extrusion
 Sheet Extrusion
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
Resin IdentificationPA612
 PA612ISO 1043
UL recognitionULDAM

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDSY5325 / 161152

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.