MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Bio-fed M·VERA® ECS1003 Engineering Biopolymer
Categories: Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Based on the technical properties shown for the M•VERA® ECS series, the following applications are possible:

Machine Construction and Tool-building:

  • Plugs
  • Housings
  • Functional parts
  • Etc..
Food Industry:
  • Packaging
  • Crates
  • Containers for liquid
  • Etc..
Sports and Leisure:
  • Gardening tools
  • Bicycle accessories
  • Etc.

Information provided by BIO-FED

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Moisture Absorption 0.550 %
@Temperature 70.0 °C,
Time 180000 sec
62 % Rel. Humidity
 1.00 %
@Temperature 70.0 °C,
Time 612000 sec
62 % Rel. Humidity
 1.30 %
@Temperature 70.0 °C,
Time 1.44e+6 sec
62 % Rel. Humidity
 
Mechanical PropertiesOriginal ValueComments
Tensile Modulus 6100 MPa
@Temperature 70.0 °C,
Time 1.44e+6 sec
Rel. humidity: 62 %
 6500 MPa
@Temperature 70.0 °C,
Time 900000 sec
Rel. humidity: 62 %
 7500 MPa
@Temperature 70.0 °C,
Time 180000 sec
Rel. humidity: 62 %
 8900 MPa
@Temperature 70.0 °C,
Time 0.000 sec
Rel. humidity: 62 %
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 80.0 °CFlange
 220 - 300 °CSector 1 – sector 4
Nozzle Temperature 240 - 295 °C
Drying Temperature 80.0 °C
@Time 14400 sec
Hold Pressure 30.0 - 80.0 MPa
Back Pressure 5.00 - 15.0 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBFED021 / 250807

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.