MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aurora Kunststoffe AUROtec® PEEK 450 natural PEEK
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: Product description: AUROtec® PEEK 450 natural is a unfilled high end performance compound, semi crystalline for injection molding

Typical applications: Gear wheels, high heat applications, metal substitution

Information provided by Aurora Kunststoffe GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.29 g/cc0.0466 lb/in³ISO 1183
Water Absorption at Saturation 0.45 %0.45 %Water; ISO 62
Viscosity 350 cP
@Temperature 400 °C
350 cP
@Temperature 752 °F
ISO11443
Linear Mold Shrinkage, Flow 0.010 cm/cm
@Temperature 180 °C
0.010 in/in
@Temperature 356 °F
60x60x2, MT; ISO 294-4
Linear Mold Shrinkage, Transverse 0.013 cm/cm
@Temperature 180 °C
0.013 in/in
@Temperature 356 °F
60x60x2, MT; ISO 294-4
Storage Temperature <= 30.0 °C<= 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 95.0 MPa13800 psi5mm/min; ISO 527-1,-2
Elongation at Yield 40 %40 %50mm/min; ISO 527-1,-2
Tensile Modulus 3.80 GPa551 ksi1mm/min; ISO 527-1,-2
Charpy Impact Unnotched NBNBISO 179-1eU
Charpy Impact, Notched 0.650 J/cm²3.09 ft-lb/in²ISO 179-1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 343 °C649 °FISO 75,-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 150 °C302 °FISO 75,-1,-2
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 355 - 375 °C671 - 707 °F
Mold Temperature 170 - 200 °C338 - 392 °F
Drying Temperature 120 - 150 °C248 - 302 °F
Dry Time 3.00 - 5.00 hour3.00 - 5.00 hour
Moisture Content <= 0.020 %<= 0.020 %Residual, Karl Fischer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAUROK226 / 249920

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.