MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Alfa Chemistry Materials Zirconium(IV) Propoxide (70% in 1-Propanol)
Categories: Fluid

Material Notes: Approx. 70% in 1-Propanol. TETRA-N-PROPYL ZIRCONATE is a yellow-colored liquid with an alcohol-like odor. Has about the same density as water and is insoluble in water. Vapors are heavier than air. May be irritating to skin, eyes, and mucous membranes.

Synonyms: zirconium(4+); A7Z4N4E80X; TR-010919; KS-000012UL; Tetra n-Propyl Zirconate; Zirconium(IV) propoxide solution; Propyl alcohol, zirconium(4+) salt; zirconium tetra propoxide; 1-Propanol, zirconium(4+) salt; UNII-A7Z4N4E80X

Smiles: CCC[O-].CCC[O-].CCC[O-].CCC[O-].[Zr+4];

Information provided by Alfa Chemistry Materials.

Vendors: Alfa Chemistry is an ISO 9001:2015 certified supplier of various materials, including: MOFs, coatings, nanomaterials, metals, polymers, carbon fibers, graphite, ceramics, glass, semiconductors, catalysts, carbon nanotubes, fullerene, COFs, molecular sieve, quantum dots, recycled plastics, photonic and optical materials, and magnetic materials, for customers worldwide. Alfa Chemistry also provides custom synthesis services for nearly all kinds of materials and chemicals. Learn more about Alfa Chemistry's high quality products at materials.alfachemic.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Molecular Weight 326.103 g/mol326.103 g/mol"Exact Mass" - Based on Specific Isotopes
 326.103 g/mol326.103 g/molMonoisotopic Mass - Isotopic Peak from Most Abundant Isotopes
 327.576 g/mol327.576 g/mol
 
Descriptive Properties
Alfa Chemistry Materials CategoryMetals and Materials
CAS Number23519-77-9
Complexity7.2
Covalently-Bonded Unit5
EC Number245-711-9
H-Bond Acceptor4
Heavy Atom Count17
InChIInChI=1S/4C3H7O.Zr/c4*1-2-3-4;/h4*2-3H2,1H3;/q4*-1;+4;
InChIKeyXPGAWFIWCWKDDL-UHFFFAOYSA-N;
IUPAC Namepropan-1-olate;zirconium(4+);
Molecular FormulaC12H28O4Zr
Rotatable Bond Count4
Topological Polar Surface Area92.2A^2
UN Number1993
UNIIA7Z4N4E80X

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

ZZALFA1296 / 268835

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.