MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Go Yen Chemical GoyenchemUV-5411 UV Absorber
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: CAS No. 3147-75-9

GoyenchemUV-5411 is an outstanding UV absorber can be used in polyethylene, polypropylene, polyurethane, polyoxymethylene, polyamides and polyester elastomer.

Applications: GoyenchemUV- 5411 is a light stabilizer can be applied on various polymer system, especially on PET, PVC, Styrene, acrylic, polycarbonate, PVB. GoyenchemUV-5411 owns broad UV absorption, with low color, low volatility and excellent solubility. GoyenchemUV- 5411 can also be used in injection / extrusion molding, plate, glass windows, automobile component and etc. GoyenchemUV-5411 light stabilizer especially for coating, light related products, sealant, elastic material.

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Ash <= 0.10 %<= 0.10 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 103 - 107 °C217 - 225 °F
 
Descriptive Properties
AppearanceWhite to slightly yellowish crystalline powder or granule
Assayby HPLC
Color>96%Color of solution (10g/100ml Toluene) 440nm
 >98%Color of solution (10g/100ml Toluene) 500nm
Loss on drying<0.3%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN524 / 266832

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.