MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Kumho-Sunny ABS722 PMMA/ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded; Acrylic (PMMA)

Material Notes: ABS722 is injection grade PMMA/ABS resin. ABS722 has high gloss, high impact, anti-scratch. ABS722 is mainly used in complex part, thin layer part, small appliance as telephone, sound, etc.

Information provided by Shanghai Kumho Sunny Plastics co, Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cmASTM D955
Melt Flow 25 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 52.0 MPaASTM D638
Elongation at Break 20 %ASTM D638
Flexural Strength 70.0 MPaASTM D790
Flexural Modulus 2300 MPaASTM D790
Izod Impact, Notched 150 J/m
@Thickness 3.20 mm
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °CASTM D648
Vicat Softening Point 96.0 °CB; ASTM D1525
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 190 - 210 °C
Middle Barrel Temperature 200 - 220 °C
Front Barrel Temperature 220 - 230 °C
Nozzle Temperature 220 - 230 °C
Melt Temperature 200 - 230 °C
Mold Temperature 40.0 - 60.0 °C
Drying Temperature 80.0 - 90.0 °C
Dry Time 3.00 - 4.00 hour
Back Pressure 1.00 - 5.00 MPa
Screw Speed 30 - 60 rpm
 
Descriptive Properties
Pencil HardnessF500g, ASTM D3363

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKMSN195 / 281047

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.