MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

EMS-Grivory Grilamid® LKN-5H Nylon 12, 50% Glass Bead Filled, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Glass Bead Filled

Material Notes: Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Filler/Reinforcement: Glass Bead, 50% Filler by Weight

Features: UV Resistant

Uses: Appliance Component; Automotive Applications; Connectors; Consumer Applications; Electrical/Electronic Applications; Household Goods; Industrial Applications; Medical Devices; Power/Other Tools

RoSH Compliance: RoSH Compliant

Forms: Granules

Processing Method: Injection Molding

Information provided by EMS-Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.44 g/cc0.0520 lb/in³ISO 1183
Water Absorption 0.40 %0.40 %Equilibrium, 50% RH; ISO 62
Water Absorption at Saturation 0.80 %0.80 %ISO 62
Linear Mold Shrinkage, Flow 0.0090 cm/cm0.0090 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 50.0 MPa7250 psiISO 527-2
Tensile Strength, Yield 50.0 MPa7250 psiISO 527-2
Elongation at Break 20 %20 %Nominal; ISO 527-2
Elongation at Yield 5.0 %5.0 %ISO 527-2
Tensile Modulus 2.60 GPa377 ksiISO 527-1
Charpy Impact Unnotched 13.0 J/cm²62.0 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched  0.399 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.504 J/cm²
@Temperature 22.8 °C
2.40 ft-lb/in²
@Temperature 73.0 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 90.0 µm/m-°C50.0 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C50.0 µin/in-°FISO 11359-2
Melting Point 178 °C352 °F10ºC/min; ISO 11357-3
Maximum Service Temperature, Air 120 °C248 °FLong Term; ISO 2578
 150 °C302 °FShort Term
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C149 °FUnannealed; ISO 75-2/A
Deflection Temperature at 8.0 MPa 40.0 °C104 °FUnannealed; ISO 75-2/C
Minimum Service Temperature, Air 90.0 °C194 °FLong Term; ISO 2578
Flammability, UL94 HB
@Thickness 0.762 mm
HB
@Thickness 0.0300 in
IEC 60695-11-10,-20

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGRIM138 / 307497

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.