MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Greene Tweed CHEMRAZ® 514 Perfluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Greene Tweed’s Chemraz® 514, a perfluoroelastomer, is a white specialty compound, perfect for applications where contamination from carbon black must be prevented. Chemraz 514 offers a Shore A hardness value of 70. Because of its wide temperature range, -22°F to 428°F (-30°C to 220°C) Chemraz 514 is ideally suited for applications ranging from mechanical seals to valves.

Available for use as O-rings, gaskets and many other custom shapes

Applications:

  • Mechanical seals
  • Pump housings
  • Reactors
  • Mixers
  • Valves
  • Couplings
  • Sprayers and dispensers

Information provided by Greene Tweed.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.12 g/cc2.12 g/ccASTM D297
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070ASTM D2240
Tensile Strength at Break 10.1 MPa1460 psiASTM D1414
Tensile Strength, Yield 2.07 MPa300 psi@ 50% Elongation; ASTM D1414
 4.69 MPa680 psi@100% Elongation; ASTM D1414
Elongation at Break 190 %190 %ASTM D1414
Compression Set 25 %
@Temperature 204 °C,
Time 252000 sec
25 %
@Temperature 400 °F,
Time 70.0 hour
At 25% deflection; ASTM D395
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 220 °C428 °F
Minimum Service Temperature, Air -30.0 °C-22.0 °F
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Kalrez® 6221 FFKM Perfluoroelastomer
DuPont Mobility and Materials Kalrez® 4079AMS FFKM Perfluoroelastomer
DuPont Mobility and Materials Kalrez® 1050LF FFKM Perfluoroelastomer
3M Dyneon™ TFE 90 Peroxide Cure Perfluoroelastomer
3M Dyneon™ PFE 80Z Peroxide Cure Perfluoroelastomer

PGREEN04 / 42298

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.