Product Description: Flame Retardant Grade. Characteristics: Flame retardant; Jet black, High gloss Availability: Asia Pacific; Europe; North America Additive: Flame Retardant Features: Flame Retardant; High Gloss Agency Rating: EC 1907/2006 (REACH) RoHS Compliance: RoHS Compliant UL File Number: E162823 Appearance: BlackInformation provided by Formosa Chemicals & Fiber Corporation |