MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ LUBRICOMP™ Compound RFL46ES Polyamide 66 (Nylon 66)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: LNP LUBRICOMP RFL46ES compound is based on Nylon 6/6 resin containing 30% glass fiber, 20% PTFE. Added features of this grade include: Wear Resistant, Heat Stabilized, Easy Molding.

Features: Wear resistant,Heat Stabilized,Easy Molding,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.55 g/cc0.0560 lb/in³ASTM D792
Moisture Absorption 0.150 - 0.250 %0.150 - 0.250 %Injection Molding
 0.430 %0.430 %23°C/50% RH/24 hrs; ASTM D570
 0.820 %0.820 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm0.0020 - 0.0050 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0090 - 0.030 cm/cm0.0090 - 0.030 in/in24hrs; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 145 MPa21000 psi5 mm/min; ISO 527
 146 MPa21200 psi5 mm/min; ASTM D638
Elongation at Break 2.6 %2.6 %5 mm/min; ASTM D638
 2.6 %2.6 %5 mm/min; ISO 527
Tensile Modulus 10.42 GPa1511 ksi1 mm/min; ISO 527
 10.88 GPa1578 ksi5 mm/min; ASTM D638
Flexural Strength 221 MPa32100 psiISO 178
 223 MPa32300 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 9.26 GPa1340 ksi2 mm/min; ISO 178
 9.28 GPa1350 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 97.0 J71.5 ft-lbASTM D256
Izod Impact, Unnotched 9.39 J/cm17.6 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 9.00 kJ/m²4.28 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 56.0 kJ/m²26.6 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 8.00 J5.90 ft-lbASTM D3763
Impact Test 2.00 J1.48 ft-lbMultiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.590.59ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.640.64ASTM D3702 Modified: Manual
K (wear) Factor 24.2 x 10-8 mm³/N-M12.0 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 31.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
17.2 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
CTE, linear, Transverse to Flow 84.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
46.7 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 251 °C484 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 251 °C
@Thickness 3.20 mm
484 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 232 °C450 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 233 °C
@Thickness 3.20 mm
451 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Zone 2 280 - 295 °C536 - 563 °F
Zone 3 295 - 305 °C563 - 581 °F
Melt Temperature 280 - 305 °C536 - 581 °FInjection Molding
Mold Temperature 95.0 - 110 °C203 - 230 °F
Drying Temperature 80.0 °C176 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80997 / 288944

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.