MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC LEXAN™ Copolymer 4504 Polycarbonate (PC) (Europe)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with biocompatibility information and should not be used for medical applications which require biocompatibility. Alternative grade HPH4504.

Features: High Heat Resistance

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183
Viscosity 10 cP
@Load 5.00 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0070 cm/cmSABIC method
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 122ISO 2039-2
Tensile Strength at Break 55.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 65.0 MPa50 mm/min; ISO 527
Elongation at Break >= 50 %50 mm/min; ISO 527
Elongation at Yield 7.0 %50 mm/min; ISO 527
Tensile Modulus 2300 MPa1 mm/min; ISO 527
Flexural Modulus 2300 MPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) 54.0 kJ/m²80*10*3; ISO 180/1A
 12.0 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*3; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*3; ISO 180/1U
Charpy Impact Unnotched NBEdgew 80*10*3 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 59.0 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 15.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.0
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.024
@Frequency 100 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.210 W/m-KISO 8302
Hot Ball Pressure Test 125 °CPASS; IEC 60695-10-2
Vicat Softening Point 160 °CRate B/120; ISO 306
Flammability, UL94 V-2
@Thickness 1.60 mm
UL 94 by SABIC-IP
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 320 - 340 °C
Zone 2 310 - 330 °C
Zone 3 320 - 340 °C
Melt Temperature 325 - 360 °CInjection Molding
Mold Temperature 100 - 125 °C
Drying Temperature 125 - 135 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
Precipitation Temperature 60.0 - 80.0 °CHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80070 / 288017

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.