MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Beryllium Cupro-Nickel, UNS C96600, Copper Casting Alloy, TF00 Temper, As Sand Cast Precipitation Hardened
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Precipitation Hardened

Casting Characteristics: High – Casting Yield, Drossing, Fluidity, Gassing, Shrinkage in Solidification; Low - Effect of Section Size

Fabrication Properties: Excellent Suitability – Soldering, Brazing; Good Suitability – Oxyacetylene Welding; Fair Suitability – Gas Shielded Arc Welding, Coated Metal Arc Welding

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.80 g/cc0.318 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 2424
Tensile Strength 827 MPa120000 psi
Tensile Strength, Yield 517 MPa75000 psi0.2% Offset
Elongation at Break 12 %12 %
Tensile Modulus 152 GPa22000 ksi
Modulus of Rigidity 57.03 GPa8271 ksiCalculated
Poissons Ratio 0.330.33
Fatigue Strength 159 MPa
@# of Cycles 1.00e+8
23000 psi
@# of Cycles 1.00e+8
Machinability 20 %20 %
Charpy Impact 55.6 J41.0 ft-lbV-Notch
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000430 ohm-cm0.0000430 ohm-cm4% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 - 300 °C
9.00 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 2.51 W/m-K17.4 BTU-in/hr-ft²-°F
Melting Point 1100 - 1180 °C2010 - 2160 °F
Solidus 1100 °C2010 °F
Liquidus 1180 °C2160 °F
Shrinkage 1.82 %1.82 %Patternmaker's Shrinkage (7/32 in./ft.)
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 °C500 °FStress Relief
Solution Temperature 982 - 1010 °C
@Time 60.0 sec
1800 - 1850 °F
@Time 0.0167 hour
Water
Precipitation Temperature 510 °C950 °FAir
 
Component Elements PropertiesMetricEnglishComments
Beryllium, Be 0.40 - 0.70 %0.40 - 0.70 %
Copper, Cu 64 - 69.8 %64 - 69.8 %As Balance
Iron, Fe 0.80 - 1.1 %0.80 - 1.1 %
Lead, Pb <= 0.010 %<= 0.010 %
Manganese, Mn <= 1.0 %<= 1.0 %
Nickel, Ni 29 - 33 %29 - 33 %
Silicon, Si <= 0.15 %<= 0.15 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC96600x1 / 293251

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.