MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC CYCOLAC™ DL100 ABS (Asia)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: CYCOLAC DL100 is a high heat, high impact, low emissions ABS/PC blend.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cmSABIC method
Melt Flow 7.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
 8.0 g/10 min
@Load 5.00 kg,
Temperature 260 °C
cm³/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 104ASTM D785
Ball Indentation Hardness 91.0 MPaISO 2039-1
Tensile Strength, Yield 44.0 MPa5 mm/min; ASTM D638
 45.0 MPa50 mm/min; ISO 527
 46.0 MPa5 mm/min; ISO 527
Elongation at Break 10 %50 mm/min; ISO 527
 60 %5 mm/min; ISO 527
 90 %5 mm/min; ASTM D638
Elongation at Yield 3.4 %50 mm/min; ISO 527
 3.5 %5 mm/min; ISO 527
Tensile Modulus 2200 MPa1mm/min; ISO 527
 2240 MPa5 mm/min; ASTM D638
Flexural Yield Strength 69.0 MPa2 mm/min; ISO 178
Flexural Modulus 2250 MPa2 mm/min; ISO 178
Izod Impact, Notched 700 J/mASTM D256
 550 J/m
@Thickness 6.40 mm
ASTM D256
Izod Impact, Notched (ISO) 35.0 kJ/m²80*10*4; ISO 180/1A
 15.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 34.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 14.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 98.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 98.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 104 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
 105 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °C1.8 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
 88.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 90.0 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 105 °CRate B/50; ISO 306
 107 °CRate B/120; ISO 306
UL RTI, Electrical 60.0 °CUL 746B
UL RTI, Mechanical with Impact 60.0 °CUL 746B
UL RTI, Mechanical without Impact 60.0 °CUL 746B
Flammability, UL94 HB
@Thickness 3.00 mm
UL 94
 HB
@Thickness 1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 80.0 °CHopper Temperature
Nozzle Temperature 245 - 275 °CInjection Molding
Zone 1 230 - 260 °C
Zone 2 250 - 280 °C
Zone 3 250 - 280 °C
Melt Temperature 250 - 280 °C
Mold Temperature 40.0 - 80.0 °C
Drying Temperature 90.0 - 100 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Moisture Content 0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10004 / 243471

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.