MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC NORYL GTX™ Resin GTX6203 Polyphenylene Ether + PA (PPE+Nylon) (Europe)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polyphenylene Ether/PPO

Material Notes: NORYL GTX™ 6203 resin is a 20% talc reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This injection moldable grade has low co efficient of thermal expansion (CTE), excellent processability, superior dimensional stability, and good surface appearance. NORYL GTX6203 resin is an excellent candidate for automotive exterior body panels.

Features: Hydrolytic Stability,Chemical Resistance,Low Creep Sensitivity,Good Stiffness,Low Warpage,Exceptional Processing,Aesthetics & Visual effects,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.25 g/cc1.25 g/ccASTM D792
Density 1.24 g/cc0.0448 lb/in³ISO 1183
Moisture Absorption 0.0700 %0.0700 %Injection Molding
 1.10 %1.10 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 3.2 %3.2 %ISO 62-1
Viscosity 20 cP
@Load 5.00 kg,
Temperature 280 °C
20 cP
@Load 11.0 lb,
Temperature 536 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0060 - 0.0090 cm/cm
@Thickness 3.20 mm
0.0060 - 0.0090 in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse 0.0060 - 0.0090 cm/cm
@Thickness 3.20 mm
0.0060 - 0.0090 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 20 g/10 min
@Load 5.00 kg,
Temperature 280 °C
20 g/10 min
@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 60.0 MPa8700 psi50 mm/min; ISO 527
 65.0 MPa9430 psi5 mm/min; ASTM D638
Tensile Strength, Yield 60.0 MPa8700 psi50 mm/min; ISO 527
 65.0 MPa9430 psi5 mm/min; ASTM D638
Elongation at Break 3.0 %3.0 %5 mm/min; ASTM D638
 10 %10 %5 mm/min; ISO 527
 10 %10 %50 mm/min; ISO 527
Elongation at Yield 2.5 %2.5 %5 mm/min; ISO 527
 3.0 %3.0 %5 mm/min; ASTM D638
Tensile Modulus 4.60 GPa667 ksi5 mm/min; ASTM D638
 4.90 GPa711 ksi1 mm/min; ISO 527
Flexural Strength 90.0 MPa13100 psiyield, 2 mm/min; ISO 178
 100 MPa14500 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 3.80 GPa551 ksi1.3 mm/min, 50 mm span; ASTM D790
 4.00 GPa580 ksi2 mm/min; ISO 178
Izod Impact Notched 60.0 J44.3 ft-lbASTM D256
 50.0 J
@Temperature -30.0 °C
36.9 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 6.00 kJ/m²2.86 ft-lb/in²80*10*4; ISO 180/1A
 5.00 kJ/m²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 50.0 kJ/m²23.8 ft-lb/in²80*10*4; ISO 180/1U
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 10.0 J7.38 ft-lbASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
33.3 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 75.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
41.7 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow  78.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
43.3 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 90.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
50.0 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
Thermal Conductivity 0.260 W/m-K1.80 BTU-in/hr-ft²-°FISO 8302
Hot Ball Pressure Test 125 °C257 °FPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 190 °C374 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
 190 °C
@Thickness 3.20 mm
374 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 185 °C365 °FRate B/50; ASTM D1525
 190 °C374 °FRate B/120; ISO 306
 190 °C374 °FRate B/50; ISO 306
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 270 - 290 °C518 - 554 °F
Zone 2 270 - 290 °C518 - 554 °F
Zone 3 280 - 300 °C536 - 572 °F
Melt Temperature 280 - 300 °C536 - 572 °FInjection Molding
Mold Temperature 80.0 - 100 °C176 - 212 °F
Drying Temperature 100 - 110 °C212 - 230 °FInjection Molding
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hourInjection Molding
Precipitation Temperature 60.0 - 80.0 °C140 - 176 °FHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82125 / 290072

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.