SABIC ULTEM™ Resin UF5011S Polyetherimide (PEI) (Europe)
Categories:
Polymer
;
Thermoplastic
;
Polyetherimide (PEI)
Material Notes:
Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming.
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.28
g/cc
1.28
g/cc
ASTM D792
Density
1.28
g/cc
0.0462
lb/in³
ISO 1183
Moisture Absorption
0.0200 %
0.0200 %
Injection Molding
0.200 %
0.200 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation
1.2 %
1.2 %
ISO 62-1
Viscosity
20
cP
@Load 5.00 kg,
Temperature 360 °C
20
cP
@Load 11.0 lb,
Temperature 680 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow
0.0040
-
0.0070
cm/cm
0.0040
-
0.0070
in/in
SABIC method
0.0040
-
0.0070
cm/cm
@Thickness 3.20 mm
0.0040
-
0.0070
in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse
0.0040
-
0.0070
cm/cm
@Thickness 3.20 mm
0.0040
-
0.0070
in/in
@Thickness 0.126 in
SABIC method
Melt Flow
11
g/10 min
@Load 6.60 kg,
Temperature 337 °C
11
g/10 min
@Load 14.6 lb,
Temperature 639 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
75.0
MPa
10900
psi
5 mm/min; ASTM D638
85.0
MPa
12300
psi
5 mm/min; ISO 527
Tensile Strength, Yield
100
MPa
14500
psi
5 mm/min; ASTM D638
100
MPa
14500
psi
5 mm/min; ISO 527
Elongation at Break
50 %
50 %
5 mm/min; ISO 527
60 %
60 %
5 mm/min; ASTM D638
Elongation at Yield
8.0 %
8.0 %
5 mm/min; ASTM D638
8.0 %
8.0 %
5 mm/min; ISO 527
Tensile Modulus
2.90
GPa
421
ksi
5 mm/min; ASTM D638
2.90
GPa
421
ksi
1 mm/min; ISO 527
Flexural Strength
110
MPa
16000
psi
yield, 2 mm/min; ISO 178
138
MPa
20000
psi
yld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus
2.90
GPa
421
ksi
2 mm/min; ISO 178
3.10
GPa
450
ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched
59.0
J
43.5
ft-lb
ASTM D256
2080
J
@Thickness 3.20 mm
1530
ft-lb
@Thickness 0.126 in
reverse notched; ASTM D256
Izod Impact, Unnotched
21.0
J/cm
39.3
ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO)
5.00
kJ/m²
2.38
ft-lb/in²
80*10*4; ISO 180/1A
5.00
kJ/m²
@Temperature -30.0 °C
2.38
ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO)
NB
NB
80*10*4; ISO 180/1U
NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched
NB
NB
Edgew 80*10*4 sp=62mm; ISO 179/1eU
NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched
0.700
J/cm²
3.33
ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
0.700
J/cm²
@Temperature -30.0 °C
3.33
ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy
30.0
J
22.1
ft-lb
ASTM D3763
Electrical Properties
Metric
English
Comments
Volume Resistivity
2.50e+15
ohm-cm
2.50e+15
ohm-cm
IEC 60093
Surface Resistance
>=
1.00e+15
ohm
>=
1.00e+15
ohm
ROA; IEC 60093
Dielectric Constant
3.2
@Frequency 50.0 - 60.0 Hz
3.2
@Frequency 50.0 - 60.0 Hz
ASTM D150
Dielectric Strength
18.0
kV/mm
@Thickness 3.20 mm
457
kV/in
@Thickness 0.126 in
in oil; ASTM D149
18.1
kV/mm
@Thickness 3.20 mm
460
kV/in
@Thickness 0.126 in
in oil; IEC 60243-1
Dissipation Factor
0.0021
@Frequency 50.0 - 60.0 Hz
0.0021
@Frequency 50.0 - 60.0 Hz
ASTM D150
0.0021
@Frequency 50.0 - 60.0 Hz
0.0021
@Frequency 50.0 - 60.0 Hz
IEC 60250
Comparative Tracking Index
100
V
100
V
IEC 60112
150
V
150
V
IEC 60112
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
55.0
µm/m-°C
@Temperature -40.0 - 150 °C
30.6
µin/in-°F
@Temperature -40.0 - 302 °F
ASTM E831
55.0
µm/m-°C
@Temperature 23.0 - 150 °C
30.6
µin/in-°F
@Temperature 73.4 - 302 °F
ISO 11359-2
CTE, linear, Transverse to Flow
55.0
µm/m-°C
@Temperature -40.0 - 150 °C
30.6
µin/in-°F
@Temperature -40.0 - 302 °F
ASTM E831
55.0
µm/m-°C
@Temperature 23.0 - 150 °C
30.6
µin/in-°F
@Temperature 73.4 - 302 °F
ISO 11359-2
Thermal Conductivity
0.310
W/m-K
2.15
BTU-in/hr-ft²-°F
ASTM C177
Hot Ball Pressure Test
125
°C
257
°F
PASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi)
208
°C
406
°F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
210
°C
410
°F
Edgew 120*10*4 sp=100mm; ISO 75/Be
213
°C
@Thickness 3.20 mm
415
°F
@Thickness 0.126 in
unannealed; ASTM D648
216
°C
@Thickness 6.40 mm
421
°F
@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
198
°C
388
°F
Flatw 80*10*4 sp=64mm; ISO 75/Af
200
°C
392
°F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
201
°C
@Thickness 3.20 mm
394
°F
@Thickness 0.126 in
unannealed; ASTM D648
204
°C
@Thickness 6.40 mm
399
°F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point
215
°C
419
°F
Rate B/120; ISO 306
215
°C
419
°F
Rate B/50; ISO 306
220
°C
428
°F
Rate A/50; ISO 306
227
°C
441
°F
Rate B/50; ASTM D1525
Processing Properties
Metric
English
Comments
Nozzle Temperature
360
-
380
°C
680
-
716
°F
Zone 2
355
-
375
°C
671
-
707
°F
Zone 3
365
-
390
°C
689
-
734
°F
Melt Temperature
365
-
390
°C
689
-
734
°F
Injection Molding
Mold Temperature
135
-
165
°C
275
-
329
°F
Drying Temperature
150
°C
302
°F
Injection Molding
Dry Time
4.00
-
6.00
hour
4.00
-
6.00
hour
Injection Molding
24.0
hour
24.0
hour
Cumulative; Injection Molding
Back Pressure
0.300
-
0.700
MPa
43.5
-
102
psi
Shot Size
40 - 60 %
40 - 60 %
Vent Depth
0.00250
-
0.00760
cm
0.000984
-
0.00299
in
Screw Speed
40
-
70
rpm
40
-
70
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PSABH82767 / 290714
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.