MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Nabaltec GRANALOX® NM 9915 B Ceramic Body, Binder Free
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Nabaltec offers ceramic bodies with different alumina content as free-of-binder grades. With the addition of necessary amount of water (approx. 20 %) these grades can be directly used for slip casting. After the application of appropriate plasticizers they are also suitable for other molding technologies (e.g. extrusion, injection molding, tape casting).

Information provided by Nabaltec.

Key Words: Al2O3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.86 - 3.94 g/cc0.139 - 0.142 lb/in³Sintered
Moisture Absorption at Equilibrium <= 0.50 %<= 0.50 %
Particle Size 160 - 220 µm160 - 220 µmMean Granulate Size
 
Processing PropertiesMetricEnglishComments
Sintering Temperature 1650 - 1750 °C3000 - 3180 °FInterval (dense ceramic parts)
 1720 °C
@Time 7200 sec
3130 °F
@Time 2.00 hour
 
Component Elements PropertiesMetricEnglishComments
Al2O3 99.7 %99.7 %
Na2O 0.10 %0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Anderman Ceramics EA99P Sintered Alumina, 99%, Porous
Alumina, alpha Al2O3, 99.5%
Zircar Zirconia ALK-15 Alumina Knit Textile Insulation
Zircar Zirconia ALF-100 Alumina Felt Insulation
Montmorillonite Al2O3-4SiO2-nH2O

CNABAL82 / 159831

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.