MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Angst+Pfister APSOplast® POM-C GF25 POM-C + 25% glass fibre
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, 30% Glass Fiber Reinforced

Material Notes: This POM copolymer, reinforced with 25 % glass fibre, is characterized by increased rigidity and strength in comparison with non-reinforced types. This can be advantageous in various applications in mechanical engineering, transport and mechanical conveying and handling, electrotechnology, precision engineering, domestic appliances, etc.

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.59 g/ccDIN EN ISO 1183-1
Water Absorption 0.070 %
@Time 86400 sec
DIN EN ISO 62
 0.20 %
@Time 346000 sec
DIN EN ISO 62
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 180 MPaDIN EN ISO 2039-1
Tensile Strength 51.0 MPa50 mm/min; DIN EN ISO 527
Tensile Strength, Yield 51.0 MPa50 mm/min; DIN EN ISO 527
Elongation at Break 12 %50 mm/min; DIN EN ISO 527
Elongation at Yield 9.0 %50 mm/min; DIN EN ISO 527
Modulus of Elasticity 4.20 GPa1 mm/min, tensile test; DIN EN ISO 527
 4.10 GPa
@Load 1.02 kg
2 mm/min, flexural test; DIN EN ISO 527
Flexural Strength 88.0 MPa
@Load 1.02 kg
DIN EN ISO 178
Compressive Strength 23.0 MPa
@Strain 1 %,
Load 1.02 kg
5 mm/min; EN ISO 604
 39.0 MPa
@Strain 2 %,
Load 1.02 kg
5 mm/min; EN ISO 604
Compressive Modulus 3600 MPa5 mm/min; EN ISO 604
Charpy Impact Unnotched 36.0 kJ/m²DIN EN ISO 179-1eU
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
DIN 53752
 80.0 µm/m-°C
@Temperature 23.0 - 100 °C
DIN EN ISO 11359-1-2
Specific Heat Capacity 1.20 J/g-°C
Thermal Conductivity 0.470 W/m-K
Melting Point 165 °CISO 11357-3
Maximum Service Temperature, Air 100 °Cshort term
 140 °Clong term
Glass Transition Temp, Tg -60.0 °CDIN 53765
Flammability, UL94 HB
@Thickness 3.00 mm
 
Descriptive Properties
Colorgreyish white

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PANGP043 / 250541

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.