MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nouryon Phospholan PE169
Categories: Other Engineering Material

Material Notes: Phospholan PE169 is a mixture of mono- and diphosphate esters based on alcohol ethoxylate in acid form

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/cc
pH 2.51% in water
Viscosity 900 cP
Surface Tension 28 dynes/cmaccording to Du Noüy, 25°C, 0.1%; DIN 53914
 
Chemical PropertiesOriginal ValueComments
Acid Value 70 - 78[mg KOH/g]
 
Thermal PropertiesOriginal ValueComments
Pour Point -10.0 °C
Flash Point >= 150 °C
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 1.0 %
 
Descriptive Properties
AppearanceClear liquid
Content (%)100Active content
Foam Height according to Ross-Miles108 mm0 ppm immediately, 50°C, 0.05%, pH 6
 56 mm300 ppm after 5 min, 50°C, 0.05%, pH 6
 78 mm0 ppm after 5 min, 50°C, 0.05%, pH 6
 83 mm300 ppm immediately, 50°C, 0.05%, pH 6
Wetting power23 secaccording to Draves, 0.1%, pH 6, 25°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY849 / 286372

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.