LNP LUBRICOMP 5CL23 compound is based on Polyvinylidene Fluoride (PVDF) resin containing 15% carbon fiber, 10% PTFE. Added features of this grade include: Wear Resistant, Electrically Conductive. Features: Light-weight Structural,Wear resistant,Electrically Conductive,Structural Information provided by SABIC |