MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Starflam® 377H NT0801 PA66 FR
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced, Flame Retardant

Material Notes: Starflam 377H NT0801 is an unfilled, PA66 homo-polymer utilizing a non-halogen flame retardant, designed with superior flow properties to assist in filling thin-walled, intricate parts. It is heat stabilized to provide best in class RTI. 377H NT0801 is also lubricated for machine feed, easy mold release and formulated with enhanced ductility.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccDAM; ISO 1183
Linear Mold Shrinkage, Flow 0.017 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.012 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 49.0 MPa50% RH; ISO 527-2
 82.0 MPaDAM; ISO 527-2
Elongation at Break 17 %DAM; ISO 527-2
 85 %50% RH; ISO 527-2
Tensile Modulus 1500 MPa50% RH; ISO 527-2
 3500 MPaDAM; ISO 527-2
Flexural Strength 43.0 MPa50% RH; ISO 178
 103 MPaDAM; ISO 178
Flexural Modulus 1700 MPa50% RH; ISO 178
 3700 MPaDAM; ISO 178
Izod Impact, Notched (ISO) 3.30 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 3.60 kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
 3.70 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 4.80 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 180/1A
 5.00 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 8.60 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched 79.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eU
 82.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 86.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 152 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eU
 160 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 NB
@Temperature 23.0 °C
50% RH; ISO 179/1eU
Charpy Impact, Notched 3.10 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eA
 3.10 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 3.10 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 4.00 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 4.30 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eA
 11.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 600 V
@Thickness 3.00 mm
IEC 60112
Hot Wire Ignition, HWI 60 - 120 secPLC 1; UL 746
 60 - 120 secPLC 1; UL 746
 
Thermal PropertiesOriginal ValueComments
Melting Point 262 °CDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 212 °CUnannealed; 50% RH; ISO 75-2/B
 228 °CUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °CUnannealed; DAM; ISO 75-2/A
 103 °CUnannealed; 50% RH; ISO 75-2/A
UL RTI, Electrical 150 °C
@Thickness 0.400 mm
UL 746
 150 °C
@Thickness 0.750 mm
UL 746
UL RTI, Mechanical with Impact 110 °C
@Thickness 0.400 mm
UL 746
 110 °C
@Thickness 0.750 mm
UL 746
UL RTI, Mechanical without Impact 130 °C
@Thickness 0.400 mm
UL 746
 130 °C
@Thickness 0.750 mm
UL 746
Flammability, UL94 V-0
@Thickness 0.400 mm
 V-0
@Thickness 0.750 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 260 - 290 °CInjection
Middle Barrel Temperature 265 - 290 °CInjection
Front Barrel Temperature 265 - 290 °CInjection
Nozzle Temperature 265 - 290 °CInjection
Melt Temperature 270 - 285 °CInjection
Mold Temperature 65.0 - 95.0 °CInjection
Drying Temperature >= 80.0 °CInjection
Dry Time >= 4.00 hourInjection
 
Descriptive Properties
AdditiveFlame Retarding Agent
 Heat Stabilizer
 Lubricant
AppearanceNatural Color
FeaturesChemical Resistant
 Corrosion Resistant
 Flame Retardant
 Good Electrical Properties
 Good Mold Release
 Good Toughness
 Heat Aging Resistant
 High Elongation
 Ignition Resistant
 Lubricated
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific
Smoke Density, Ds Max123EN ISO 5659-2
Smoke Toxicity, CITNLP0.61NF X 70-100-1/2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASCE9107 / 287558

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.