GOYENCHEM-DE420 is GO YEN CHEMICAL INDUSTRIAL CO., LTD. (GYC Group) Dep. Of Technical invent for majority of copper and metal for corrosion protection, which is synthetic nano structures water based metal corrosion inhibitor. While applying GOYENCHEMDE420 on metals, it will form a transparent thin membrane evenly on the surface that can be the protection layer from corrosion by air and harmful materials. It is mainly use for metal yellow color protection, preventing the corrosion of cobalt alloys as well as applying on black metal. Applications: - Non-ferrous metal Copper and copper alloys
- Protection of metal and retard corrosion
- Prevent the metal from the environment atmosphere
- Protection of metal corrosion by water and harmful media
- Metal yellow color protection
- Delay cobalt alloy corrosion
- Can be use on ferrous metals
- Freezing
- Engine coolant
Information provided by Go Yen Chemical |