MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Konson Magnesium Stearate for PVC Heat Stabilizer
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product name: Magnesium stearate

Molecular formula: Mg[CH3(CH2)16COO]2

Magnesium stearate is a kind of tiny, light and white powder with greasy touch sense, insoluble in water, ethanol neither ethoxyethane, but soluble in hot water, hot ethanol, decomposes into stearic acid and magnesium salts when contacting with acid.

Application: Magnesium stearate is widely adopted in food, medicine, paint, plastic, rubber and textile fields and mainly function as emulsifier, releasing agent, lubricant, stabilizer, or accelerant etc. Also it can be used as stabilizer and lubricant in PVC or ABS resin etc.

Information provided by Konson®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.100 - 0.350 g/cc
Particle Mesh Size 325 Mesh>99%
 
Thermal PropertiesOriginal ValueComments
Melting Point 110 °C
 
Component Elements PropertiesOriginal ValueComments
Magnesium, Mg 4.0 - 5.0 %
 
Descriptive Properties
Appearancetiny, light and white powder
Content<1%Free Acid
Loss of Drying=0.5%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKONS067 / 256112

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.