MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Osterman & Co Osterlene® LD6521 LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Product Description: LD6521 is a general purpose LDPE grade resin. It has good toughness and stiffness and is easy to process. Applications for LD6521 include domestic housewears, food containers, rigid medium sized moldings, film applications, non-abrasive packaging applications

Availability: North America
Features: General Purpose; Good Processability; Good Stiffness; Good Toughness; Medium Rigidity
Uses: Film; Food Containers; General Purpose; Household Goods; Packaging

Information provided by Osterman & Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.921 g/ccASTM D1505
Melt Flow 6.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 48ASTM D2240
Tensile Strength at Break 1500 psiASTM D638
Film Elongation at Break, MD 320 %ASTM D882
Film Elongation at Break, TD 380 %ASTM D882
Elongation at Yield 13 %ASTM D638
Tensile Modulus 32000 psiASTM D638
Flexural Modulus 49300 psiASTM D790
Secant Modulus, MD 30.0 ksiASTM D790
Secant Modulus, TD 37.0 ksiASTM D882
Dart Drop Test 50.0 gASTM D1709
Film Tensile Strength at Break, MD 2880 psiASTM D882
Film Tensile Strength at Break, TD 2180 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 201 °FASTM D1525
Brittleness Temperature -45.4 °FF50; ASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

POSTER079 / 267661

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.