MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Poly Alloy Etoma™ ET1201 PP with Carbon Black
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with Carbon Black Filler

Material Notes: Etoma ET1201 resin is a conductive compound based on polypropylene with carbon black. ET1201 is designed specific to sheet extrusion with extension during process. The sheet still keeps excellent mechanical properties and conductivity. It will be a perfect solution for electrical conductive straps

Information provided by Poly Alloy Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.03 g/ccASTM D792
Melt Flow 0.10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 380 kg(f)/cm²ASTM D638
Elongation at Break 7.0 %ASTM D638
Flexural Strength 9250 psiASTM D790
Flexural Modulus 27000 kg(f)/cm²ASTM D790
Izod Impact, Notched 2.50 kg-cm/cmASTM D256
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square <= 1000 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 135 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 74.0 °CASTM D648
Shrinkage 1.1 - 1.5 %ASTM D955
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 205 - 215 °C
Middle Barrel Temperature 205 - 225 °C
Front Barrel Temperature 205 - 225 °C
Nozzle Temperature 190 - 210 °C
Mold Temperature 60.0 - 70.0 °C
Drying Temperature 120 °C
Dry Time 4.00 - 8.00 hour
Shelf Life 24.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPALLOY024 / 278303

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.