MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Toyobo Riteflex® 430 Thermoplastic Copolyester Elastomer
Categories: Polymer; Thermoplastic; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes: Product Description: Riteflex 430 is a nominal 30 Shore D thermoplastic polyester elastomer with low modulus and outstanding low temperature impact and tear resistance.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Uses: Coating Applications; Film; Sheet

Form: Pellets

Processing Method: Coating; Film Extrusion; Extrusion; Injection Molding; Sheet Extrusion

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/ccISO 1183
Water Absorption at Saturation 0.70 %ISO 62
Maximum Moisture Content 0.050
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 30
@Time 15.0 sec
ISO 868
Tensile Strength at Break 2900 psiISO 527-2/50
Elongation at Break 700 %ISO 527-2/50
Flexural Modulus 3630 psiISO 178
Izod Impact, Notched (ISO) NBISO 180/1A
Izod Impact, Unnotched (ISO) NBISO 180/1U
Charpy Impact Unnotched NBISO 179/1eU
Charpy Impact, Notched NBISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 338 °FISO 11357-3
 
Processing PropertiesOriginal ValueComments
Processing Temperature 68.0 - 122 °FHopper
 338 - 374 °FHot Runner
Rear Barrel Temperature 311 - 338 °F
Middle Barrel Temperature 338 - 356 °F
Front Barrel Temperature 338 - 356 °F
Nozzle Temperature 338 - 374 °F
Melt Temperature 338 - 374 °F
Mold Temperature 68.0 - 131 °F
Drying Temperature 212 - 230 °F
Dry Time 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHCQ6314 / 311007

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.