MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ STAT-KON™ Compound DEL329EP Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP STAT-KON DEL329EP compound is based on Polycarbonate (PC) resin containing 10% carbon fiber, 15% PTFE, Flame Retardant. Added features of this grade include: Electrically Conductive, Internally Lubricated, Flame Retardant, Wear Resistant.

Features: Internally Lubricated,Light-weight Structural,Super Strong (Carbon Fiber Filled),Flame Retardant,Wear resistant,Electrically Conductive

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 g/cc0.0488 lb/in³ISO 1183
Water Absorption 0.22 %
@Time 86400 sec
0.22 %
@Time 24.0 hour
ISO 62-1
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/inSABIC method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 103 MPa14900 psi5 mm/min; ISO 527
Elongation at Break 1.6 %1.6 %5 mm/min; ISO 527
Tensile Modulus 8.60 GPa1250 ksi1 mm/min; ISO 527
Flexural Strength 143 MPa20700 psiyield, 2 mm/min; ISO 178
Flexural Modulus 7.20 GPa1040 ksi2 mm/min; ISO 178
Flexural Strain at Break 2.5 %2.5 %2 mm/min; ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²2.86 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 20.0 kJ/m²9.52 ft-lb/in²80*10*4; ISO 180/1U
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 100 - 10000 ohm100 - 10000 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 18.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
10.0 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 82.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
45.6 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 144 °C291 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 140 °C284 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
UL RTI, Electrical 80.0 °C176 °FUL 746B
UL RTI, Mechanical with Impact 80.0 °C176 °FUL 746B
UL RTI, Mechanical without Impact 80.0 °C176 °FUL 746B
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Zone 2 310 - 320 °C590 - 608 °F
Zone 3 320 - 330 °C608 - 626 °F
Melt Temperature 305 - 325 °C581 - 617 °FInjection Molding
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81231 / 289178

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.