MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC CYCOLOY™ FR C6600 PC+ABS (Europe)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: CYCOLOY C6600 Polycarbonate/Acrylonitrile Butadiene Styrene (PC/ABS) blend is an injection moldable non chlorinated/brominated flame retardant grade with balanced flow, impact and hydrolytic stability. It also offers good chemical resistance and colorability in opaque colors. It has a UL94 V0@1.5mm and 5VB@2.0mm flame rating.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ISO 1183
Water Absorption 0.60 %0.60 %23°C/sat; ISO 62
Moisture Absorption 0.200 %0.200 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inSABIC method
Melt Flow 16 g/10 min
@Load 2.16 kg,
Temperature 260 °C
16 g/10 min
@Load 4.76 lb,
Temperature 500 °F
cm³/10 min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 122122ISO 2039-2
Ball Indentation Hardness 110 MPa16000 psiISO 2039-1
Tensile Strength at Break 50.0 MPa7250 psi50 mm/min; ISO 527
Tensile Strength, Yield 60.0 MPa8700 psi50 mm/min; ISO 527
Elongation at Break >= 50 %>= 50 %50mm/min; ISO 527
Elongation at Yield 4.0 %4.0 %50 mm/min; ISO 527
Tensile Modulus 2.70 GPa392 ksi1mm/min; ISO 527
Flexural Yield Strength 90.0 MPa13100 psi2 mm/min; ISO 178
Flexural Modulus 2.70 GPa392 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²7.14 ft-lb/in²80*10*4; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NBNB80*10*4; ISO 180/1U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched NBNBEdgew 80*10*4 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 1.50 J/cm²7.14 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant  2.7
@Frequency 50.0 - 60.0 Hz
2.7
@Frequency 50.0 - 60.0 Hz
IEC 60250
 2.7
@Frequency 1e+6 Hz
2.7
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength  17.0 kV/mm
@Thickness 3.20 mm
432 kV/in
@Thickness 0.126 in
in oil; IEC 60243-1
 25.0 kV/mm
@Thickness 1.60 mm
635 kV/in
@Thickness 0.0630 in
in oil; IEC 60243-1
 35.0 kV/mm
@Thickness 0.800 mm
889 kV/in
@Thickness 0.0315 in
in oil; IEC 60243-1
Dissipation Factor  0.0040
@Frequency 50.0 - 60.0 Hz
0.0040
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.0060
@Frequency 1e+6 Hz
0.0060
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 250 - 400 V250 - 400 VUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
41.7 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow  75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
41.7 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°FISO 8302
Hot Ball Pressure Test 75.0 °C167 °FIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C194 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °F1.8 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 95.0 °C203 °FRate B/50; ISO 306
 107 °C225 °FRate B/120; ISO 306
UL RTI, Electrical 80.0 °C176 °FUL 746B
UL RTI, Mechanical with Impact 70.0 °C158 °FUL 746B
UL RTI, Mechanical without Impact 80.0 °C176 °FUL 746B
Flammability, UL94  V-2
@Thickness 0.750 mm
V-2
@Thickness 0.0295 in
UL 94
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
UL 94
 5VB
@Thickness 2.00 mm
5VB
@Thickness 0.0787 in
UL 94
Oxygen Index 32 %32 %ISO 4589
Glow Wire Test  775 °C
@Thickness 1.00 mm
1430 °F
@Thickness 0.0394 in
IEC 60695-2-13
 960 °C
@Thickness 1.00 mm
1760 °F
@Thickness 0.0394 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Processing Temperature 60.0 - 80.0 °C140 - 176 °FHopper Temperature
Nozzle Temperature 250 - 270 °C482 - 518 °FInjection Molding
Zone 1 230 - 250 °C446 - 482 °F
Zone 2 240 - 260 °C464 - 500 °F
Zone 3 250 - 270 °C482 - 518 °F
Melt Temperature 250 - 270 °C482 - 518 °F
Mold Temperature 70.0 - 85.0 °C158 - 185 °F
Drying Temperature 80.0 - 90.0 °C176 - 194 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10787 / 244254

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.