MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

GRECO ISOTANE® 2090A-M Poly(caprolactone) ester, TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Characteristics: ISOTHANE® 2000 series products are poly(caprolactone) ester based thermoplastic polyurethane. They exhibit excellent mechanical properties, hydrolysis resistance, oil resistance and outstanding low compression set. ISOTHANE® 2000 series can be injection molded and extruded.

Application: Seals, Gaskets and Mechanical Items

Information provided by Great Eastern Resins Industrial Co. Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9191ASTM D2240
Tensile Strength 56.0 MPa8120 psiASTM D412
Elongation at Break 450 %450 %ASTM D412
50% Modulus 9.00 MPa9.00 MPaASTM D412
100% Modulus 11.0 MPa1600 psiASTM D412
300% Modulus 26.0 MPa3770 psiASTM D412
Tear Strength 120 kN/m685 pliDie C; ASTM D624
Compression Set  20 %
@Temperature 23.0 °C,
Time 79200 sec
20 %
@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
 28 %
@Temperature 70.0 °C,
Time 79200 sec
28 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGRECO5183 / 282166

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.